Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Quantum PEEK 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Parker Chomerics THERM-A-FORM T642 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Parker Chomerics THERMATTACH® T421 Thermally Conductive BGA Assembly Tape
THERMATTACH have been designed to provide a high performance bond in the assembly of EBGA and TBGA semiconductor packages. Their thermally conductive filler ensures superior package performance whe..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D 792
RTP Company RTP 303 TFE 20 SE Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-0
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Celanese Celanex® 4306 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.30% glass-fiber, impact modified, low warpInformation provided by Celanese
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
RTP Company RTP 4085 TFE 20  Polyphthalamide (PPA) Carbon Fiber 30% - PTFE 20%  (discontinue
Carbon Fiber 30% - PTFE 20%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D 792
RTP Company RTP 399 X 93608 Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Perfluoropolyether Oil - Flame Retardant
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D 792
RTP Company RTP 881 TFE 15 Acetal (POM), Carbon Fiber Reinforced - PTFE Lubricated
Specific Gravity 1.50 g/cc
1.50 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant
Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66
G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon.
Specific Gravity 1.50 - 1.56 g/cc
1.50 - 1.56 g/cc
NBR NM-IEC 60811-1-3
Karina E 42/6-FC-LMP Red Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Specific Gravity 1.50 g/cc
1.50 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1301-7896 PPS, linear, with carbon fiber, thermally conductive modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Stiff parts, low coefficient of..
Specific Gravity 1.50 g/cc
1.50 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL
LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant.
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D 792
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
Specific Gravity 1.50 g/cc
1.50 g/cc
Trelleborg Commercial Neoprene® C798 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Specific Gravity 1.50 g/cc
1.50 g/cc
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Specific Gravity 1.50 g/cc

@Temperature 23.0 °C
1.50 g/cc

@Temperature 73.4 °F
ASTM D792
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Specific Gravity 1.50 g/cc
1.50 g/cc
mixed, uncured
Atom Adhesives AA-CARB 61 Epoxy Adhesive
AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and me..
Specific Gravity 1.50 g/cc
1.50 g/cc
@ 25°C
ACC EP MAP-Z 18 EPI Engineered Polymers Aliphatic Polymer
EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail..
Specific Gravity 1.50 - 1.56 g/cc
1.50 - 1.56 g/cc
ASTM D 792
Karina 800-36/395-CY-RT Brown PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D 792
RTP Company RTP 2299 X 113763 B Polyetheretherketone (PEEK), Carbon Fiber - Aramid Fiber - PTFE Lubricated - Perfluoropolyether Oil
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D 792
RTP Company RTP 802 SI 2 DEL Acetal (POM), Glass Fiber - Silicone Lubricated - Homopolymer
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
RTP Company RTP 203B GB 20 TFE 10 HS UV  Nylon 6/10 (PA 6/10) Glass Fiber 20% - Glass Bead 20% - PTFE 10% - Heat Stable - UV Stable