Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 3.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
11.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
11.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.9 MPa
7960 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 4.3 %
4.3 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.487 GPa
360.7 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.335 J/cm

@Thickness 3.17 mm
2.501 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 108 °C

@Load 1.00 kg,
Thickness 3.17 mm
226 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1527
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in