Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers DIAMALOY PCPBT 2525 PC/PBT Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY PCPBT 2525 PC/PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 265 °C
24 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.4 MPa
8620 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 3.8 %
3.8 %
chs 2.0 in/min; ASTM D638
Flexural Strength 85.8 MPa
12400 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.184 GPa
316.8 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 138 °C

@Load 1.00 kg,
Thickness 3.17 mm
280 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525