Polymer Property : Tensile Strength, Yield = 8620 psi
Polymer Property :
Tensile Strength, Yield =
8620 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
59.4
MPa
8620
psi
chs 2.0 in/min; ASTM D638
Diamond Polymers DIAMALOY PCPBT 2525 PC/PBT Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.