Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP25-0715CF20 20% Conductive Filler Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-0715CF20 20% Conductive Filler Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Filler Content 20 %
20 %
ASTM D5630
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 100 %
100 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.459 GPa
356.6 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256