Diamond Polymers NPP30-2000HC Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP30-2000HC Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 40.7 MPa
5900 psi
chs 50 mm/min; tangent; ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
chs 1.3 mm/min; 1% secant; ASTM D790
Izod Impact, Notched 0.182 J/cm
0.341 ft-lb/in
ASTM D256