Material Notes:
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.890 - 0.910 g/cc
0.890 - 0.910 g/cc
ASTM D792
Melt Flow 4.5 - 7.5 g/10 min

@Temperature 230 °C
4.5 - 7.5 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 29.0 MPa
4210 psi
ASTM D790
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648