Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.899 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D648
Users viewing this material also viewed the following: