Diamond Polymers Softflex® SF 5591 Thermoplastic Vulcanizate (TPV)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® SF 5591 Thermoplastic Vulcanizate (TPV).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.027 - 0.029 cm/cm

@Thickness 3.17 mm
0.027 - 0.029 in/in

@Thickness 0.125 in
Direction of Flow; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.20 MPa
464 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 415 %
415 %
chs 2.0 in/min; ASTM D638
Compression Set 30 %

@Temperature 25.0 °C,
Time 79200 sec
30 %

@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0580 in