Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.027 - 0.029 cm/cm @Thickness 3.17 mm |
0.027 - 0.029 in/in @Thickness 0.125 in |
Direction of Flow; ASTM D955 |
Diamond Polymers Softflex® SF 5591 Thermoplastic Vulcanizate (TPV) Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |