Dow AFFINITY™ EG 8100G Ethylene-octene copolymer

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ EG 8100G Ethylene-octene copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY™ EG 8100G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene-octene copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance clarity, sealability and toughness of the structure.Information provided by Dow
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Mooney Viscosity 23.6

@Temperature 121 °C
23.6

@Temperature 250 °F
ML 1+4; ASTM D1646
Melt Flow 1.0 g/10 min
1.0 g/10 min
Melt Flow Ratio = 7.6 (I<sub>10</sub>/I<sub>2</sub>); ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
ASTM D2240
Tensile Strength, Ultimate 10.60 MPa
1537 psi
ASTM D638
Tensile Strength, Yield 1.71 MPa
248 psi
ASTM D638
6.12 MPa
887 psi
100% Secant; ASTM D638
Elongation at Break 1115 %
1115 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 55.0 °C
131 °F
Dow Method
Vicat Softening Point 42.8 °C
109 °F
ASTM D1525