Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow AFFINITY™ VP 8770 Polyolefin Plastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ VP 8770 Polyolefin Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® VP 8770 polyolefin plastomer is an alpha-olefin resin for general purpose applications. It exhibits excellent optics and flexibility. Its low specific gravity can help control resin and production costs, while reducing the weight of end products.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.885 g/cc
0.0320 lb/in³
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Strength, Ultimate 22.1 MPa
3210 psi
Tensile Strength, Yield 3.20 MPa
464 psi
Elongation at Break >= 1000 %
>= 1000 %
Tensile Modulus 0.0221 GPa
3.21 ksi
Users viewing this material also viewed the following: