Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Innovene 1088 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: General purposeTypical applications: Water quenched blown filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3045 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Compression; Injection moldingFeatures: Medium-term heat aging; UL recognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05M-00 Polypropylene Homopolymer Grade H05M-00 is a general purpose polypropylene homopolymer for injection molding applications. This resin provides good long-term heat stability. This material meets the requirements of the Food.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H20H-00 Polypropylene Homopolymer This resin is designed to provide easy moldability for applications requiring resistance to long term heating. This material has been recognized by UL for sustained use at 130c.Suggested fabricatio.. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.885 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 701 Series 40 Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and econ.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP) AFFINITY™ EG 8185 Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a lower density POP polymer exhibiting high elasticity for fibers.Information provided by Dow |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Density | 0.885 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 701 Series 40 Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and econ.. |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | |
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Density | 0.887 g/cc | 0.0320 lb/in³ | |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.887 g/cc | 0.0320 lb/in³ | |
BASF N,N-Dimethylethanolamine Formula: C4H13NOCAS: 108-01-0Description: N,N-Dimethylethanolamine S is a colorless to slightly yellow liquid with an amine-like odor. It is miscible in water.Synonyms: DMEA, DMEOA, Dimethylamine-2.. |
|||
Density | 0.885 g/cc @Temperature 23.0 °C |
0.0320 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18390 Maleic Anhydride Modified Polyethylene OREVAC® 18390 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9346 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9934 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, Antistatic, High surface hardness, Stain resistanceComplies with FDA specification, Title 21, CFR 177.1520.Typica.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9965 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3240 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Fiber Optic CableFeatures: NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Density | 0.886 - 1.84 g/cc | 0.0320 - 0.0665 lb/in³ | Average value: 0.918 g/cc Grade Count:172 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 0.886 - 1.46 g/cc | 0.0320 - 0.0527 lb/in³ | Average value: 0.906 g/cc Grade Count:153 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8649X Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Developmental Grade. Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Low taste/odor, Excellent processabilityTypical applications: High clarity c.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8939 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Excellent static control, ToughenedTypical applications: Housewares, Rigid packaging, Media packag.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 6361 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |