Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow C133-02 Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Blow Molding Grade , Polypropylene, Impact Modified; Molded/Extruded , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C133-02 Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewDow C133-02 Polypropylene Resin is intended for use in extrusion, thermoforming, and extrusion blow molding applications where impact at refrigeration temperatures is desired. It is especially suited for corrugated profile extrusion applications.High impactGood stiffnessComplies with: U.S. FDA 21 CRF 177.1520(c) 3.2a, Canadian HPFB No ObjectionDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790A
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: