Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus, 1% Secant = 1240 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1240 MPa

@Temperature 23.0 °C
180000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Ineos H03G-04 Polypropylene Homopolymer
This is a polypropylene homopolymer for biaxially oriented polypropylene (BOPP) film and blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as ..
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790
ExxonMobil HD 6719.17 Injection Molding Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790
ExxonMobil HD 6719.62 Injection Molding Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790B
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790B
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790A
Dow C133-02 Polypropylene Impact Copolymer Resin
OverviewDow C133-02 Polypropylene Resin is intended for use in extrusion, thermoforming, and extrusion blow molding applications where impact at refrigeration temperatures is desired. It is especia..
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM-D790
Braskem GP100OR HDPE High Density Extrusion Polyethylene
GP100OR is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal technology and has high molar mass. It s..