Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow C7014-35RNA Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C7014-35RNA Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW™ C7014-35RNA Polypropylene Resin is a high impact copolymer intended for injection molding processes. It is especially suited for thin-wall flow path molds.Main CharacteristicsFast set-upEasy mold fillingEasy mold releaseContains an antistatic and nucleating additiveComplies WithU.S. FDA FCN 843HPFB (Canada), No ObjectionDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus, 1% Secant 1030 MPa
149000 psi
ASTM D790A
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Unannealed; ASTM D648