Material Notes:
Dow Polypropylene Impact Copolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resistance and ESCR; excellent moisture barrier; good gloss; good impact over wide range of temperature and low water absorption. Dow Polypropylene Impact Copolymer resins are suitable for a wide range of applications and may be fabricated by injection molding, blow molding and extrusion. C702-20 Polypropylene Impact Copolymer resin is suitable for injection molding.Data provided by Dow Chemical.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM Data
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 230 °C
19 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM Data
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
Unannealed; ASTM Data