Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19 g/10 min | 19 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5210 PC+ABS (Europe-Africa-Middle East) CYCOLOY CY5210 is a flame retardant PC/ABS using non-chlorinated and non-brominated FR additives for injection moulding. CYCOLOY CY5210 has an improved hydrolytic stability with balanced flow and im.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific) 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin
(discontinued **) Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® SLD3000 PC (Asia Pacific) Antistatic colorable/opaque FR PC grade |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Lehmann & Voss LUVOCOM® 80-7626 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Ineos ABS Lustran® ABS 150G10 10% Glass Fiber Reinforced Grade |
|||
Melt Flow | 19 g/10 min @Load 6.60 kg, Temperature 337 °C |
19 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 250 °C |
19 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GW-1041 PC/ABS, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Melt Flow | 19 g/10 min @Load 3.80 kg, Temperature 230 °C |
19 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 360 °C |
19 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem LTX931A PEI Blend (Europe-Africa-Middle East) Post-industrial recycle based, 30% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Bright White P80514PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80514PF is a bright white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and molding .. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Bright White P80514PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80514PF is a bright white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and molding .. |
|||
Melt Flow | 19 g/10 min | 19 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 350 Ethylene Vinyl Acetate DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: .. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
|
Covestro Bayblend® R-T 60 Polycarbonate/ABS Blend Recycled grade in which carefully reclaimed old parts and production rejects and/or scrap from all processes of manufacturing or processing undergo material recycling. Slightly decreased impact stre.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 1954 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosity• UV st.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Clariant Renol TES3050A Thermoplastic Elastomer Alloy Data provided by Clariant Masterbatches |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® DP 6015 Polycarbonate + PBT Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical .. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® DP 7102 000000 PBT, 30% Mineral
(discontinued **) PBT, 30% mineral, injection molding, LDS |