Dow Corning 1248 Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 1248 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone glycol graft copolymer with secondary hydroxyl functionality. The polymer has a combination of organoreactivity from the glycol group as well as properties typical of a polydimethylsiloxane fluid. The glycol group can be chemically bonded into any system which is reactive towards alcohols to impart durable silicone properties to that system.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Viscosity Measure 160 cSt
160 cSt
kinetic/kinematic
Surface Tension 2.15 dynes/cm
2.15 dynes/cm
Thermal Properties Metric English Comments
Pour Point -85.0 °C
-121 °F
Flash Point >= 100 °C
>= 212 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.411
1.411
Processing Properties Metric English Comments
Shelf Life 30.0 Month
30.0 Month
Descriptive Properties Value Comments
Active Content (%) >95
Color Clear, Hazy
Hydrophobic Yes