Dow Corning 1437 INDUSTRIAL SEALANT AND ADHESIVE

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 1437 INDUSTRIAL SEALANT AND ADHESIVE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neutral Cure RTV SealantInformation provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 21
21
Tensile Strength, Ultimate 0.896 MPa
130 psi
Tensile Strength, Yield 0.414 MPa
60.0 psi
at 150% elongation, maximum
Elongation at Break 300 %
300 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 22.0 °C
24.0 hour

@Temperature 71.6 °F
Shelf Life 12.0 Month
12.0 Month