Material Notes:
High molecular weight silicone dispersion in water.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Volatiles 20 %
20 %
Thermal Properties Metric English Comments
Flash Point 94.0 °C
201 °F
closed cup
Descriptive Properties Value Comments
Color Translucent