Material Notes:
A 10% dispersion of high molecular weight silicone polyether in cyclopentasiloxane fluid for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications. INCI Name: Cyclopentasiloxane (and) PEG/PPG-18/18 DimethiconeInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.956 g/cc

@Temperature 25.0 °C
0.956 g/cc

@Temperature 77.0 °F
Viscosity Measure 100 - 6000 cSt
100 - 6000 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 77.0 °C
>= 171 °F
Closed cup
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (%) <94
Nonvolatile Content (%) 10.5