Dow Corning 7091 ADHESIVE SEALANT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 7091 ADHESIVE SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance, neutral cure silicone adhesive/sealant.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc

@Temperature 25.0 °C
1.40 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 37
37
Tensile Strength, Ultimate 2.50 MPa
363 psi
Elongation at Break 680 %
680 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color Black
Grey
White