Dow Corning PH-1555 HRI Cosmetic Fluid

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning PH-1555 HRI Cosmetic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A trimethyl pentaphenyl trisiloxane which provides ultra high refractive index for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications.INCI Name: Trimethyl Pentaphenyl TrisiloxaneInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.092 - 1.099 g/cc

@Temperature 25.0 °C
1.092 - 1.099 g/cc

@Temperature 77.0 °F
Viscosity Measure 175 cSt
175 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 101.1 °C
>= 214.0 °F
Closed cup
243 °C
469 °F
Open cup
Optical Properties Metric English Comments
Refractive Index 1.5775 - 1.58
1.5775 - 1.58