Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 175 cSt | 175 cSt | kinetic/kinematic |
Dow Corning 705 DIFFUSION PUMP FLUID A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning |
|||
Viscosity Measure | 175 cSt | 175 cSt | Kinetic/Kinematic |
Dow Corning PH-1555 HRI Cosmetic Fluid A trimethyl pentaphenyl trisiloxane which provides ultra high refractive index for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications.INCI Name: Trimeth.. |