Dow Corning SE 4490 CV

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SE 4490 CV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.62 g/cc

@Temperature 25.0 °C
2.62 g/cc

@Temperature 77.0 °F
Viscosity <= 500000 cP
<= 500000 cP
Dynamic
Thermal Properties Metric English Comments
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Strength 3.94 kV/mm
100 kV/in
Processing Properties Metric English Comments
Shelf Life 10.3 Month
10.3 Month
Descriptive Properties Value Comments
Color White
Hydrophobic Yes
Nonflowable Yes
Water Resistant Yes