Polymer Property : Dielectric Strength = 100 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 3.94 kV/mm
100 kV/in
Short Term; ASTM D149
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet)
Dielectric Strength 3.94 kV/mm
100 kV/in
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u..
Dielectric Strength 3.94 kV/mm
100 kV/in
Garlock THERMA-PURâ„¢ 4122-KAMM High Temperature Gasketing Material
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u..
Dielectric Strength 3.94 kV/mm
100 kV/in
ASTM D149
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum
Information provided by ITW Devcon
Dielectric Strength 3.94 kV/mm
100 kV/in
Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive
TRA-BOND 2122 is a versatile aluminum metal filled epoxy formulation developed for modern industrial casting, bonding and repair applications where a strong aluminum-like adhesive is required. This ..
Dielectric Strength 3.94 kV/mm
100 kV/in
Dow Corning SE 4490 CV
One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning
Dielectric Strength 3.94 kV/mm
100 kV/in
Cotronics Duralco™ 4540 Machinable Epoxy
Patches, fills, seals, and repairs with outstanding adhesion, ductility, thermal conductivity and shock resistance.Corrosion Resistance: excellent resistance to chemicals and solventsApplications: ..
Dielectric Strength 3.94 kV/mm
100 kV/in
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength
Dielectric Strength 3.94 kV/mm
100 kV/in
Cotronics Resbond™ 918 High Temperature Ceramic Adhesive, One Composition
Dielectric Strength 3.94 kV/mm
100 kV/in
ASTM D149
Devcon HVAC Repair (Special F) Epoxy
General Repair EpoxyComments: Aluminum-filled epoxy adhesive, conveniently packaged in two 6.5 oz. tubes. Bonds to aluminum and other metals, ceramics, wood, concrete or glass. Use as an adhesive ..
Dielectric Strength 3.94 kV/mm
100 kV/in
35% RH
3M Novec™ 1710 Electronic Grade Coating
3M™ Novec™ 1710 Electronic Grade Coating is a higher solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 10 wt% fluorochemical acrylic polymer carried i..
Dielectric Strength 3.94 kV/mm
100 kV/in
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate
Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventio..
Dielectric Strength 3.94 kV/mm
100 kV/in
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia
Two-part, quick-set ceramic for small parts.
Dielectric Strength >= 3.94 kV/mm
>= 100 kV/in
3M Scotch-Seal™ 1252 Tamper Proof Sealant
3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme..
Dielectric Strength 3.94 kV/mm
100 kV/in
ASTM D149
3M 4508 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Dielectric Strength 3.94 kV/mm
100 kV/in
35% RH
3M Novec™ 1702 Electronic Grade Coating
3M™ Novec™ 1702 Electronic Grade Coating is a lower solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 0.2 wt% fluorochemical acrylic polymer carried i..
Dielectric Strength 3.94 - 15.7 kV/mm
100 - 400 kV/in
Average value: 13.1 kV/mm Grade Count:6
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
Dielectric Strength 3.94 kV/mm
100 kV/in
Garlock THERMA-PUR™ 4122-FC High Temperature Gasketing Material
THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a uniqu..