Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® 37085-V SILICONE RUBBER BLACK

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 37085-V SILICONE RUBBER BLACK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc

@Temperature 25.0 °C
1.16 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Ultimate 6.60 MPa
957 psi
Tensile Strength, Yield 1.40 MPa
203 psi
at 100% elongation, maximum
Elongation at Break 381 %
381 %
Tear Strength 11.2 kN/m
64.0 pli
Descriptive Properties Value Comments
Color black
Users viewing this material also viewed the following: