Material Notes:
30 Durometer, 2-part, 1 to 1 mix, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc

@Temperature 25.0 °C
1.12 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 8.000 MPa
1160 psi
Elongation at Break 800 %
800 %
Tear Strength 20.025 kN/m
114.23 pli
Compression Set 18 %
18 %
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance opaque
Mix Ratio (X:1) 100
Base to Catalyst ETN
Water Resistant yes