Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | >= 4320 min @Temperature 25.0 °C |
>= 4320 min @Temperature 77.0 °F |
|
ACC QLE 1030 QSI Quantum Silicones 27 Durometer Addition Cure Elastomer for Coating
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, 100%solid, fast cure.Applications: fabric or cloth coating. Part of the Amber Chem.. |
|||
Pot Life | 4320 - 5760 min | 4320 - 5760 min | (3-4 days) |
Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy TRA-DUCT 925M01 is a low ion snap cure silver-filled epoxy. TRA-DUCT 925M01 develops strong, durable, void free electrically and thermally conducting bonds. The product can be screen printed, stenci.. |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning HV 1520/40 40 Shore Hardness Conductive liquid silicone rubber with high tear strength, high electrical conductivity and fast cure speedInformation provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning HV 1520/50 KIT PARTS A&B 50 Shore Hardness injection moldable liquid silicone rubber with high tear strength, high elongation and a fast cure speedInformation provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9220/55 KIT PARTS A&B 55 Durometer, 2-part, 1 to 1 mix, black Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9251/45 A&B KIT 45 Durometer, 2-part, 1 to 1 mix, off-white, Fabric Coating grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9252/150P A&B KIT 35 Durometer, 2-part, 10 to 1 mix, translucent, Fabric Coating grade, Liquid Silicone RubberInformation provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9252/900P PARTS A&B Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9280/60E KIT PARTS A&B 75 Shore A hardness, two-part, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9280/70E KIT PARTS A&B 70 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquide Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9280/75E KIT PARTS A&B 60 Durometer, 2-part, 1 to 1 mix, translucent, injection moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9414/50E KIT PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9416/50 KIT PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® LSR 9390-40 PARTS A&B 40 Durometer, 2-part, 1 to 1 mix, off-white, molding grade, Liquid Silicone RubberInformation provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® LSR 9390-50 PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, off-white, injection molding grade, Liquid Silicone RubberInformation provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® LSR 9390-60 PARTS A&B 60 Durometer, 2-part, 1 to 1 mix, oil resistant, tan Liquid Silicone Rubber for injection molding.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-8 is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a higher viscos.. |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil.. |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping Product Description: EPO-TEK® H20S is a modified version of EPO-TEK® H20E, designed primarily for die stamping and dispensing techniques for chip bonding. EPO-TEK®H20S is a highly reliable, two .. |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® H31LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31LV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electron.. |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9252/500P PARTS A&B Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Dow Corning SILASTIC® 9416/20E KIT PARTS A&B 30 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Pot Life | 4320 min | 4320 min | |
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-LV is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a .. |
|||
Pot Life | <= 4320 min @Temperature 25.0 °C |
<= 4320 min @Temperature 77.0 °F |
100 g |
Armstrong X-6/E Epoxy Adhesive Thixotropic.Information provided by Ellsworth Adhesives. |
|||
Pot Life | 4320 min | 4320 min | (3 days) |
Abatron AboCast 8502-7/AboCure 8502-7 Colorless, Low-Exotherm Epoxy Casting Compound AboCast 8502-7/AboCure 8502-7 is a rigid, heat cured, colorless, low-exotherm epoxy casting compound for larger masses. It is a 2-component structural and dielectric liquid system with extremely low.. |
|||
Pot Life | 4320 - 5760 min | 4320 - 5760 min | (3-4 Days); working life |
Abatron Primkote 8006-1 All Purpose Epoxy Primer Primkote 8006-1 is an all purpose epoxy primer that excels as a primer for concrete, metal, and wood. It also performs well as a penetrating primer for weathered wood, concrete sealer, conditioner f.. |