Material Notes:
Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellent clarity and flexibility for low modulus applications. Its low specific gravity (density) delivers lighter weight parts. The product form is free-flowing pellets.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Melt Index of Compound <= 2.0 g/10 min

@Load 2.00 kg,
Temperature 190 °C
<= 2.0 g/10 min

@Load 4.41 lb,
Temperature 374 °F
ASTM D1238
22.5 g/10 min

@Load 10.0 kg,
Temperature 190 °C
22.5 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
10 sec; ASTM D2240
Tensile Strength, Ultimate 7.20 MPa
1040 psi
ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
100% Modulus 0.000370 GPa
0.0537 ksi
No units reported, assumed to be 37 MPa
2% Secant Modulus 0.0110 GPa
1.60 ksi
ASTM D790
Users viewing this material also viewed the following: