Material Notes:
DOW H110-02N is intended for use in extrusion and thermoforming processes. It is especially suited for applications where improved melt strength and clarity are desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min

@Temperature 230 °C
2.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa
5100 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 9.0 %
9.0 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.507 J/cm
0.950 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
0.320 J/cm

@Temperature 0.000 °C
0.600 ft-lb/in

@Temperature 32.0 °F
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 161 °C
322 °F
Dow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648
Optical Properties Metric English Comments
Haze 14 %
14 %
40 mil injection molded plaque; ASTM D1003