Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ASTM D648 |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | |
Polycasa Acryl® G 88 Acrylic Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC K5025 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ASTM D648 |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ASTM D648-97 |
Ipiranga Petrochem PH 1721 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ISO 75 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ISO 75 |
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437M20CL Mica Reinforced Coupled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | |
BASF Procom® D 1146 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | |
BASF Procom® D 1165 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |