Dow Prevail® 3100 ABS + Polyurethane

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyurethane Alloy , Polyurethane, TP
Manufacturer Dow Chemical
Trade Name Prevail®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Prevail® 3100 ABS + Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used for applications ranging from flexible bumper fascias to sports equipment components. It is easy to process and is paintable without the need for a primer.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 MPa
4000 psi
ASTM Data
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM Data
Elongation at Break 200 %
200 %
ASTM Data
Elongation at Yield 28 %
28 %
ISO Data
Tensile Modulus 0.496 GPa
71.9 ksi
ASTM Data
Izod Impact, Notched NB
NB
ASTM Data
7.48 J/cm

@Temperature -50.0 °C
14.0 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
ISO Data, Low Temp
10.0 J/cm²
47.6 ft-lb/in²
ISO Data
Impact Test 51.4 J

@Temperature 23.0 °C
37.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
65.5 J

@Temperature -30.0 °C
48.3 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
Unannealed; ASTM Data
92.0 °C
198 °F
Annealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
Unannealed; ASTM Data
75.0 °C
167 °F
Annealed; ASTM Data
Vicat Softening Point 101 °C
214 °F
Optical Properties Metric English Comments
Gloss 76 %
76 %
Gardner Gloss, 60°