Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 60 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 60 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resistance, and will not brittle with age. Used for food applications where ambient temperature swings create fogging problems in the package. It is ideally suited to overwrap fresh food products, including sausage, poultry, fish, and other trayed meat products.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM 1249
Water Vapor Transmission 24.0 g/m²/day
1.55 g/100 in²/day
ASTM 1249
Oxygen Transmission 306 cc-mm/m²-24hr-atm
777 cc-mil/100 in²-24hr-atm
or 20400 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 %
150 %
Average; ASTM D882
Modulus of Elasticity 0.190 GPa
27.6 ksi
(stiffness), ASTM D882
Coefficient of Friction, Dynamic 0.30
0.30
ASTM D1894
Seal Strength 2300 g/25 mm
2300 g/in
F-88-68(73)
Film Tensile Strength at Break, MD 76.0 MPa
11000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
Gloss 110 %
110 %