Physical Properties Metric English Comments
Moisture Vapor Transmission 0.360 - 0.750 cc-mm/m²-24hr-atm
0.914 - 1.90 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer
Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Moisture Vapor Transmission 0.360 - 0.750 cc-mm/m²-24hr-atm
0.914 - 1.90 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer
High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resista..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® RS900 Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, permeable antifog shrink film engineered for food packaging. It forms tight, leak-resistant heat seals. Printable grades (RST900) offer ..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Moisture Vapor Transmission 0.360 - 3.10 cc-mm/m²-24hr-atm
0.914 - 7.87 cc-mil/100 in²-24hr-atm
Average value: 1.13 cc-mm/m²-24hr-atm Grade Count:26
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..