Material Notes:
Elvaloy® AC 34035 is a copolymer of ethylene and butyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC 34035 resin complies with the U.S. Food and Drug Administration regulation 21CFR175.105; Adhesives, for use as a component of articles intended for use in contact with food. These resins must be separated from contact with food by a suitable functional barrier, and the quantity of adhesive which contacts fatty and aqueous foods shall not exceed the trace amount at seams and edges. This resin also complies with U.S. Food and Drug Administration regulation 21CFR176.180; Components of paper and paperboard in contact with dry food, for use as a component of the uncoated or coated food-contact surface of paper and paperboard in contact with dry food (food type VIII, identified in 21CFR176.170(c), Table 1).
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792, ISO 1183
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 90.0 °C
194 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F
Feed Temperature 135 °C
275 °F
Extrusion Coating
Zone 2 160 °C
320 °F
Extrusion Coating
Zone 3 185 °C
365 °F
Extrusion Coating
Zone 4 210 °C
410 °F
Extrusion Coating
Zone 5 210 °C
410 °F
Extrusion Coating
Adapter Temperature 210 °C
410 °F
Extrusion Coating
Die Temperature 210 °C
410 °F
Extrusion Coating
Melt Temperature 160 - 235 °C
320 - 455 °F
Extrusion Coating