Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Feed Temperature = 135 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 135 - 140 °C
275 - 284 °F
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th..
Feed Temperature 135 - 150 °C
275 - 302 °F
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification
The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D799 Sealing Resin
DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
Feed Temperature 135 °C
275 °F
Cast Film/Sheet Processing
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
Feed Temperature 135 °C
275 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Feed Temperature 135 °C
275 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Feed Temperature 135 °C
275 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Feed Temperature 135 °C
275 °F
Extrusion Coating
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Feed Temperature 135 °C
275 °F
Blown Film Extrusion
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate
Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Feed Temperature 135 °C
275 °F
Extrusion Coating
DuPont™ Elvaloy® AC34035 Ethylene Methyl Acrylate
Elvaloy® AC 34035 is a copolymer of ethylene and butyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate
DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® ..
Feed Temperature 135 °C
275 °F
Cast Film/Sheet Processing
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate
DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® ..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid
Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
Feed Temperature 135 °C
275 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
Feed Temperature 135 °C
275 °F
Extrusion Coating
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate
Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®..
Feed Temperature 135 - 150 °C
275 - 302 °F
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1706 Zinc Ionomer
Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1825 Zinc Ionomer
Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp..
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
DuPont™ Surlyn® 2601B Sodium Ionomer
Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer ..