Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range without the need for plasticizers.Elvax resins can be used alone or to improve the flexibility, resilience and toughness of other resins. Depending on the demands of the particular application, they can be pigmented, foamed, filled, and/or crosslinked. In addition to their performance advantages, Elvax resins are processed easily using conventional thermoplastic processing techniques, i.e., injection molding, extrusion and foaming, as well as rubber processing techniques, i.e., Banbury mixing, foam extrusion and molding.Test specimens except for tensile impact where prepared by compression molding (ASTM D1928, procedure C). Tensile impact samples were injection molded.Processing Information:Molding and ExtrudingModified and unmodified Elvax resins can be processed in conventional thermoplastic and rubber processing equipment. The temperature profile will vary with machine type, size and screw design as well as with part size, thickness or confiation.CompoundingElvax resins are compatible with a variety of other resins and elastomers including polyethylene, polypropylene and styrene-butadiene rubber. Clays and other inorganic fillers can be added to improve abrasion resistance and lower cost.Foaming AgentsElvax resins are readily foamed using chemical or physical blowing agents.Crosslinking AgentsPeroxides such as "Di-Cup"† and "Vul-Cup"† dicumyl peroxide can be used to crosslink or vulcanize Elvax resins.(†Hercules Inc.) Information provided by DuPont.
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM D792
Vinyl Acetate Content 18 %
18 %
TGA
Melt Index of Compound 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Hardness, Shore D 39
39
ASTM D2240
Tensile Strength, Ultimate 19.0 MPa
2760 psi
Type IV, crosshead speed 2 in/min; ASTM D638
8.30 MPa

@Temperature 49.0 °C
1200 psi

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
33.0 MPa

@Temperature -20.0 °C
4790 psi

@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
Elongation at Break 750 %
750 %
Type IV, crosshead speed 2 in/min; ASTM D638
500 %

@Temperature -20.0 °C
500 %

@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
800 %

@Temperature 49.0 °C
800 %

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
Modulus of Elasticity 0.0500 GPa
7.25 ksi
0.172 GPa

@Temperature -20.0 °C
24.9 ksi

@Temperature -4.00 °F
Flexural Modulus 0.0480 GPa
6.96 ksi
ASTM D790
0.0230 GPa

@Temperature 49.0 °C
3.34 ksi

@Temperature 120 °F
ASTM D790
0.216 GPa

@Temperature -20.0 °C
31.3 ksi

@Temperature -4.00 °F
ASTM D790
Flexural Stiffness 50.00 MPa
7252 psi
172.0 MPa

@Temperature -20.0 °C
24950 psi

@Temperature -4.00 °F
Tensile Impact Strength 505 kJ/m²
240 ft-lb/in²
At -20°C; ASTM D1822
630 kJ/m²
300 ft-lb/in²
At 23°C; ASTM D1822
Compression Set 50 %
50 %
Method B, 10 days at 25°C; ASTM D395
90 %

@Temperature 70.0 °C
90 %

@Temperature 158 °F
Method B, 22 hours; ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D762
Processing Properties Metric English Comments
Processing Temperature 121 - 204 °C
250 - 399 °F
Descriptive Properties Value Comments
Cycle time 0.5-2 minutes
Molding, equipment and part design dependent
Vinyl Acetate Content 18 wt.%
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved