Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.941 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil ESCOR™ AT 310 Extrusion Coating Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® CL-200YNR JN (Natural) Rotational molding crosslinkable high density polyethylene
(d Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 720.92 Specialty Film Resin
(discontinued **) Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® UL 7620 Adhesive Application Resin
(discontinued **) Escorene Ultra UL 7620 is a medium flow rate, 24% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids.Data provided by the manufacturer. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep.. |
|||
Density | 0.941 - 0.947 g/cc | 0.0340 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 7746 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | |
Lord Adhesives Flocklok® 851 Flock Adhesive Flocklok® 851 is a moisture curing, polyurethane flock adhesive used to adhere flock to SBR, thermoplastic elastomers, and plastic (i.e., ABS). Thermoplastic elastomers will require the use of a .. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | LE 4437; ASTM D792 |
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | LE 4437; ASTM D792 |
Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D 792 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM-D1505 |
Westlake EMAC® Plus SP1501 20% EMA Copolymer Westlake EMAC� Plus SP1501 is a 20% EMA copolymer designed for extrusion coating, compounding, and blending where low viscosity, flexibility, and strength are important. SP1501 provides excelle.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2207 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2207 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficient of friction.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2220 is a 20% EMA copolymer designed for compounding, extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00218CC3 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 240°C (464°F) may cause resin degradation.Availability: Africa & M.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2027G Linear Low Density Polyethylene For high speed, thin gauge applications Improved stiffness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 720.62 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE) ASPUN™ 6811A Fiber Grade Resin: Suggested Optimum Process: Spun Bond Typical Application: Non-woven FabricsInformation provided by Dow |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b.. |