Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range without the need for plasticizers.Elvax resins can be used alone or to improve the flexibility, resilience and toughness of other resins. Depending on the demands of the particular application, they can be pigmented, foamed, filled, and/or crosslinked. In addition to their performance advantages, Elvax resins are processed easily using conventional thermoplastic processing techniques, i.e., injection molding, extrusion and foaming, as well as rubber processing techniques, i.e., Banbury mixing, foam extrusion and molding.Test specimens except for tensile impact where prepared by compression molding (ASTM D1928, procedure C). Tensile impact samples were injection molded.Processing Information:Molding and ExtrudingModified and unmodified Elvax resins can be processed in conventional thermoplastic and rubber processing equipment. The temperature profile will vary with machine type, size and screw design as well as with part size, thickness or confiation.CompoundingElvax resins are compatible with a variety of other resins and elastomers including polyethylene, polypropylene and styrene-butadiene rubber. Clays and other inorganic fillers can be added to improve abrasion resistance and lower cost.Foaming AgentsElvax resins are readily foamed using chemical or physical blowing agents.Crosslinking AgentsPeroxides such as "Di-Cup"† and "Vul-Cup"† dicumyl peroxide can be used to crosslink or vulcanize Elvax resins.(†Hercules Inc.) Information provided by DuPont.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Vinyl Acetate Content 15 %
15 %
TGA
Melt Index of Compound 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ASTM D2240
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength, Ultimate 19.0 MPa
2760 psi
Type IV, crosshead speed 2 in/min; ASTM D638
12.0 MPa

@Temperature 49.0 °C
1740 psi

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
32.0 MPa

@Temperature -20.0 °C
4640 psi

@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
Elongation at Break 650 %
650 %
Type IV, crosshead speed 2 in/min; ASTM D638
500 %

@Temperature -20.0 °C
500 %

@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
750 %

@Temperature 49.0 °C
750 %

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
Modulus of Elasticity 0.0960 GPa
13.9 ksi
0.345 GPa

@Temperature -20.0 °C
50.0 ksi

@Temperature -4.00 °F
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
0.0530 GPa

@Temperature 49.0 °C
7.69 ksi

@Temperature 120 °F
ASTM D790
0.503 GPa

@Temperature -20.0 °C
73.0 ksi

@Temperature -4.00 °F
ASTM D790
Flexural Stiffness 96.00 MPa
13920 psi
345.0 MPa
50040 psi
Tensile Impact Strength 425 kJ/m²
202 ft-lb/in²
At -20°C; ASTM D1822
450 kJ/m²
214 ft-lb/in²
At 23°C; ASTM D1822
Compression Set 52 %
52 %
Method B, 10 days at 25°C; ASTM D395
84 %

@Temperature 70.0 °C
84 %

@Temperature 158 °F
Method B, 22 hours; ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 °C
176 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D762
Processing Properties Metric English Comments
Processing Temperature 121 - 204 °C
250 - 399 °F
Descriptive Properties Value Comments
Cycle time 0.5-2 minutes
Molding, equipment and part design dependent
Vinyl Acetate Content 15 wt.%