Mechanical Properties Metric English Comments
Flexural Modulus 0.0530 GPa
7.69 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-720 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p..
Flexural Modulus 0.0530 GPa

@Temperature 49.0 °C
7.69 ksi

@Temperature 120 °F
ASTM D790
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..