Material Notes:
A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailability: North AmericaInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792 - ISO 1183
Melt Index of Compound 1.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240 - ISO 868
Tensile Strength at Break 2.76 MPa
400 psi
ASTM D638 - ISO 527-2
Elongation at Break 550 %
550 %
ASTM D638 - ISO 527-2
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Tear Strength 17.5 kN/m
100 pli
ASTM D624