Polymer Property : Tear Strength = 17.5 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 17.5 kN/m
100 pli
NuSil R4-1140 Silicone One Part Sealing & Adhesive
General Purpose: One Part Sealing & AdhesiveComments: AdhesiveCure System: AcetoxyInformation provided by NuSil
Tear Strength 17.5 kN/m
100 pli
Typical
NuSil MED-1011 Silicone, One Part Adhesive/Sealant - Restricted Medical Use
Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and pla..
Tear Strength 17.5 kN/m
99.9 pli
ASTM D624
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
Tear Strength 17.5 kN/m

@Temperature 23.0 °C,
Time 7200 sec
99.9 pli

@Temperature 73.4 °F,
Time 2.00 hour
ASTM D624
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To..
Tear Strength 17.5 kN/m
99.9 pli
ASTM D624
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tear Strength 17.5 kN/m
100 pli
Certified
NuSil MED-2041 Dispersion - Restricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Tear Strength 17.5 kN/m
100 pli
Typical
NuSil MED4-4115 Silicone, One Part High Consistent Elastomer - Restricted Medical Use
Description: HCRs can be used for extrusion of tubing and profiles (rod or ribbon), in calendared sheeting for die-cutting, or in compression or transfer molded parts such as balloons, gaskets or o-..
Tear Strength 17.5 kN/m
99.9 pli
ASTM D624
PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To..
Tear Strength 17.5 kN/m
100 pli
ASTM D624
Kraton® G7705 GI-B (SEBS) Compound
Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Tear Strength 17.5 kN/m
99.9 pli
ASTM D624
Multibase Multi-Flex® TPE 6568 C 1 NATURAL
This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. The moisture content is 1%. The fogging test value is 70% according to ASTM GM 9305P. Multi-F..
Tear Strength 17.5 kN/m
100 pli
ASTM D624
Multibase Multi-Flex® A 4001 LC Black TPE Thermoplastic Elastomer
Features: Heat Resistance, HighOzone ResistantCompression Set, Low Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase
Tear Strength 17.5 kN/m
100 pli
ASTM D624
Multibase Multi-Flex® A 4001 LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, GoodCompressive Strength, GoodHeat Resistance, MediumOzone ResistantThermal Stability, GoodForms:PelletsProcessing Methods:Injection MoldingExtrusion Information pro..
Tear Strength 17.5 kN/m
100 pli
Initial Tear Strength
Saint-Gobain CHR® SGC6-04(R) CHEMLAM Copper Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 17.5 kN/m
100 pli
Fabric Break
Saint-Gobain COHRlastic® 300AR Reinforced Silicone Sponge/Aggressive Acrylic Adhesive Pressure Sensitive Tape
Description: Strip-N-Stick® tape provides all the benefits of silicone rubber in an easy-to-apply, pressure-sensitive adhesive tape form. Compressible and flexible, it can conform to irregular su..
Tear Strength 17.5 kN/m
100 pli
Initial Tear Strength; ASTM D624, Die B
Saint-Gobain COHRlastic® CF1867 Thermally Conductive Silicone Coated Fabric
Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. CF1867..
Tear Strength 17.5 kN/m
100 pli
Initial Tear Strength; ASTM D624, Die B
Saint-Gobain COHRlastic® Furo 407 Thermally Conductive Silicone Coated Fabric
Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. Furo 4..
Tear Strength 17.5 kN/m
100 pli
Initial Tear Strength; ASTM D624, Die B
Saint-Gobain COHRlastic® Furo 409 Thermally Conductive Silicone Coated Fabric
Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. Furo 4..
Tear Strength 17.5 kN/m
100 pli
Trouser; ASTM D470
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am..
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D 624
RTP Company RTP 2740 S-40A Saturated Styrenic Block Copolymer, General Purpose
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D 624
RTP Company RTP 2740 S-40A Z Saturated Styrenic Block Copolymer, FDA Compliant Ingredients
Tear Strength 17.5 kN/m
100 pli
ASTM D624
DuPont Keldax® 6798 Filled Thermoplastic Ethylene Polymer
A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil..
Tear Strength 17.5 kN/m
100 pli
Silicone Property; ASTM D624
Arlon CP-RC-3918 Silicone Bulk Compound
This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Tear Strength 17.5 kN/m
100 pli
cured 72 hrs @ RT
ACC QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material
QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin ..
Tear Strength 17.5 kN/m
100 pli
Typical
NuSil MED-1511 Silicone, One part Adhesive - Unrestricted Medical Use
Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and pla..
Tear Strength 17.5 kN/m
100 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® IT 086LFR Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Flame RetardantMulti-Purpose Thermoplastic ElastomerApplications:General PurposeInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Co..
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D 624
RTP Company EMI 2862-60A Value-added Thermoplastic Polyolefin Elastomer, Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D624
RTP Company RTP 2800 B-60A FR Thermoplastic Vulcanizate Elastomer, Flame Retardant  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D624
RTP Company RTP 2800 B-70A Z Thermoplastic Polyolefin Elastomer, FDA Compliant Ingredients  (discontinued **)&
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D 624
RTP Company RTP 2899 X 107551 Olefinic Thermoplastic Elastomer (TEO), Nylon 6 Overmolding
A 65 Shore A thermoplastic elastomer designed for overmolding onto nylon 6 substrates.