Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Nucrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins.Features/Benefits: Excellent adhesion to unprimed foil, paper, and metallized film. Provides substrate protection for improved structure reliability and barrier integrity. Can be extruded at low temperatures for insurance against off-tastes, off-odors, and taste/odor complaints. Low seal initiation temperature allows higher speed packaging. Good hot tack, sealability through contamination, and heat seal strength provide strong, reliable heat seals.Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous nonfood pouches and sachets. Snack structures. Other foil, metallized film, or paper coatings as a heat seal or tie layer.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 78.0 °C
172 °F
Freezing Point via DSC/ASTM D3418
97.0 °C
207 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 79.0 °C
174 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 290 °C
554 °F
Typical Die Temp.
Melt Temperature 250 - 305 °C
482 - 581 °F
Users viewing this material also viewed the following: