Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 988PA NC010 Acetal (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nucleated Low Viscosity Acetal Homopolymer with Low Screw DepositInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 190 °C
21 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
Elongation at Yield 12 %
12 %
ISO 527-1/-2
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-1/-2
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code POM
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
North America
South and Central America
Resin Identification POM
ISO 1043
UL recognition UL