Material Notes:
Delrin® SC631 is a medium-high viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 73.0 MPa

@Temperature 23.0 °C
10600 psi

@Temperature 73.4 °F
ISO 527
Elongation at Yield 16 %

@Temperature 23.0 °C
16 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 3.30 GPa

@Temperature 23.0 °C
479 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Appearance Natural Color
Features Creep Resistance, Good
Dimensional Stability, Good
Dimensional Stability, Good
Fatigue Resistant
Homopolymer
Impact Resistance, Good
Stiffness, High
Strength, High
Viscosity, Medium-high
Forms Pellets
Generic Acetal (POM) Homopolymer
Material Status Current
Part Marking Code >POM<
ISO 11469
Processing Method Extrusion
Injection Molding
Product Category Healthcare Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification POM
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Gears
Medical Applications
Parts, Engineering
Tubing