DuPont Performance Polymers Hypalon® CP-826 Adhesion Primer, General Description  (discontinued **)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hypalon® CP-826 Adhesion Primer, General Description  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hypalon CP 826 is a chlorinated, maleic anhydride grafted polypropylene resin.Suggested End Uses: Adhesion primer for:PolypropylenePolypropylene blends with TPOs (auto bumpers)Polyurethane foam, (athletic shoe construction)EVA with high levels of PE (athletic shoes)Main Features: Hypalon CP 826 has been developed to have excellent adhesion to polypropylene and blends containing polypropylene. It can be used in dilute solutions as a wash primer or tie layer between materials that are difficult to adhere. It can also be used as an adhesion modifier for coatings, adhesives and inks because of its solubility in commonly used solvents. Hypalon CP 826 is offered in solid form.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Viscosity 260 cP
260 cP
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 30.0 °C
86.0 °F
Optical Properties Metric English Comments
Gardner Color Number <= 1.0
<= 1.0
at 20% in Xylene
Descriptive Properties Value Comments
Chlorine Content 30 wt%
Product Form Chips
Saponification number 16.5 mg KOH/g