Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® 70G35NOX BK309 is a 35% glass reinforced, polyamide 66 resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa

@Temperature 23.0 °C
20300 psi

@Temperature 73.4 °F
5mm/min; 50%RH; ISO 527
220 MPa

@Temperature 23.0 °C
31900 psi

@Temperature 73.4 °F
5mm/min; DAM; ISO 527
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
5mm/min; DAM; ISO 527
5.0 %

@Temperature 23.0 °C
5.0 %

@Temperature 73.4 °F
5mm/min; 50%RH; ISO 527
Tensile Modulus 8.30 GPa

@Temperature 23.0 °C
1200 ksi

@Temperature 73.4 °F
50%RH; ISO 527
12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact Unnotched 8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
DAM; ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 295 °C
563 °F
DAM; Optimum; Injection Molding
285 - 305 °C
545 - 581 °F
DAM; Injection Molding
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM; Injection Molding
100 °C
212 °F
DAM; optimum; Injection Molding
Drying Temperature 80.0 °C
176 °F
DAM; Injection Molding
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM; Injection Molding
Moisture Content <= 0.20 %
<= 0.20 %
DAM; Injection Molding
Descriptive Properties Value Comments
Generic PA66
DAM
Product Category Glass Reinforced Resins
DAM
Copyright © lookpolymers.com All Rights Reserved