Mechanical Properties Metric English Comments
Tensile Modulus 12.0 GPa

@Temperature -40.0 °C
1740 ksi

@Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided ..
Tensile Modulus 12.0 GPa

@Temperature 60.0 °C
1740 ksi

@Temperature 140 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 12.0 GPa

@Temperature 90.0 °C
1740 ksi

@Temperature 194 °F
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 12.0 GPa

@Temperature 120 °C
1740 ksi

@Temperature 248 °F
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 12.0 GPa

@Temperature 150 °C
1740 ksi

@Temperature 302 °F
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; ..
Tensile Modulus 12.0 GPa

@Temperature 60.0 °C
1740 ksi

@Temperature 140 °F
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab..
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66
Zytel® 70G35NOX BK309 is a 35% glass reinforced, polyamide 66 resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution.Information provided by DuP..